En1.chinaelong.com is a professional manufacture of refractories in china. Our mainly refractory products are used for EAF, steel ladle, tundish and metallurgy.
Wednesday, November 13, 2013
Semi-graphitic Carbon Block
Semi-graphitic Carbon Block
It
is mad of high temperature' electrical calcined anthracite as main a
material, medium temperate pitch as binder, through forming, high
temperature baking, final precision machining.
It features good thermal conductivity and alkaline resistance.
It is economic and practical, and mainly applied for blast furnace bottom.
Tuesday, November 12, 2013
Mullite Insulating Firebrick
Mullite Insulating Firebrick
This series of products adopt high-purity raw materials and unique technology to furthest avoid impact of impurities and structure defect to product performance, featuring in extreme excellent high-temperature volume stability, thermal shock resistance, high strength, low heat conductivity coefficient, with extensive adaptability to various furnace types and environment conditions. This product can be used as furnace lining (away from erosion of fusion liquid) and insulating layer in many industries like metallurgy, machinery, ceramics and chemicals, which is an ideal energy-saving product.
This series of products adopt high-purity raw materials and unique technology to furthest avoid impact of impurities and structure defect to product performance, featuring in extreme excellent high-temperature volume stability, thermal shock resistance, high strength, low heat conductivity coefficient, with extensive adaptability to various furnace types and environment conditions. This product can be used as furnace lining (away from erosion of fusion liquid) and insulating layer in many industries like metallurgy, machinery, ceramics and chemicals, which is an ideal energy-saving product.
Construction of Refractory Castable
During the construction of refractory castable, special
attention should be paid on pin welding, asphalt brushing, stirring of castable
with water, making and fixing of mould, vibration and ramming of castable,
demoulding, sizes’ and measuring points’ accuracy, etc. http://www.yilongrefractory.comDo construction strictly as material manufacturer and boiler works required.
1. Installation of Pin and Claw Nails
Reinstall the pins missing for any
reason and the pins in the area of heating surface composite melding junction
before hydraulic pressure. Lengthen
and reinstall the pins properly in coal mouth, material return mouth and upper inflection
point of air duct furnace so that meets the required density of pins. Brush all
the pre-buried metal parts and claw nails with asphalt paint (thickness > 1mm) or cover them with combustibles
before casting.
2. Dosing and Stirring of Castable & Water
The dosing of castable and water
should be done strictly as the instructions of material manufacturer. The water
should be clean, such as drinking water, ph 6-8. The mixer should be clean forced
action mixer, and clean it for the
next time using. Pay attention on the adding order of castable and water and
its stirring time, adding water freely and prolonging of stirring time are forbidden.
The water and castable should be mixed evenly and stirred till smooth. Carry
away the mixed casatble immediately after stirring, the castable poured out
from stirring tank is disallowed to be poured into the tank and stirred again.
Clean the tank after every construction for the next using, record the amount
of water and castable, and the stirring time.
3. Checking Before Making Template
Check carefully whether the pin, hook
nail and strutting part conform to the drawing, whether all the re-welding and
is done and firm, whether the temporary
metal parts have been cut off. Check whether the metal parts which should be
brushed with asphalt paint meet the requirement, whether the casting place is
clean, any other unrelated materials are forbidden to appear. For easy
demoulding, a thin tier of partition (such as used
oil) can be brushed in the mould. There can not be gaps between each two
templates to avoid castable leaking out, so that also convenient for mould
releasing. The refractory castable should be used up in 30 minutes after
stirring, and should be casted to the required thickness in 1 time. Ram the
castable till tight. For the too thick parts, cast tier by tier, while casting
the upper tier, vibration bar can not touch the lower casted tier.
Sunday, November 10, 2013
The Ways to Protect Refractories and Improve Service Life of Lalde
The
MgO in slag is eroded usually by furnace lining while making steel. In the
process of smelting, the slag and refractory materials will get touched; MgO
concentration in slag should almost reach saturation. There is a close
relationship between the content of saturated MgO and CaO/SiO2. For
slag with low alkalinity (CaO/SiO2<2.0), the higher the proportion of FeO
is, the lower proportion of saturated MgO. When FeO content is low and saturated
MgO content is high, the slag will erode more refractories. While for slag with
high alkalinity (CaO/SiO2 >2.0), the saturated MgO content will
not be seriously affected by the FeO content, what’s more the slag will not
erode much more refractories. Therefore, improve slag alkalinity can strongly
protect refractories.
The service life of ladle is directly influenced by refining
time, so it is important to improve steelmaking technology so that to shorten
smelting time.
The service life of ladle will be reduced by 3-5 heats
once shut down, so to achieve efficient production, the key is shortening
smelting cycle. On the premise of using advanced technology to guarantee the
best steel quality and the lowest total consumption, shorten the smelting cycle
to the minimum, improve equipment and shorten shut down time.
Checker Brick ,High Alumina Checker Brick,Refractory Brick,Firebrick
Checker Brick
Introduction
High Aluminum checker brick include high refractoriness, large volume density, high intensity and high refractoriness under load. They also have good creeping in high-temperature, excellent regenerative capability.Lining Material,Furnace Lining Material,Lining Material Refractory,Refractory Material,Refractorty Products
Lining Material
This
company lining material produces the lining material is called "mixed sand" for short.
This product is the main refractories of the medium frequency induction
furnace used by the small steel enterprises. Its effect is in leading
position