Firebrick
occurs burst when experiencing thermal shock, the simple reason there is
expansion and contraction, and the reason is prone to burst firebrick type
as
follows:
1.The refractory brick
is composed of mineral quartz, tridymite, cristobalite composition, the
temperature change is accompanied by a transformation of the crystalline form of
the quartz, resulting mutations volume, thermal shock so that the refractory
bricks easily burst.
Magnesia
or magnesia-chrome brick, due to the thermal expansion coefficient, thermal
firebrick
burst
prevention
1.The
use of insulating firebrick, insulating firebrick with insulation due to the
role of firebrick inside low stability, not easy to
burst.
2.To
avoid thermal shock, slow heating and cooling can be effective in preventing
refractory bricks burst.
3.Select
the heat transfer coefficient is relatively high, toughness good bricks, can
reduce the probability of bursting.